Product Description
1Black Finish Inconel738LC K438 Nickel Alloy Round Bar
2. Material Grade:
Inconel600/601/625/718/X-750/713C,
Incoloy800H/800/901/925/926/A286
Hastelloy B/B-2/C-4/C-22/C-276,
Monel400/K500,Nickel200/201
N02200/N02201/N04400/N05500/N06600/N06601/
N06625/N06690/N07718/N07750/N08800/N08810/
N08825/N09925/N10001/N10665/N06455/N06022/
N10276/N06200/N08020/S66286/K93600/N08367/N06059/N08904.
MP35N.etc
3.Standard: ASTM BS JIS NF DIN GB
4.Size: for the hot rolled bar, 8mm-100mm
For the forged bar, 70mm-400mm
5.Length: 500--6000mm,or other length as the customers' requirements.
6.Process: hot rolled, forged, cold drawn
7.Surface: black surface, polished surface
![Casting Superalloy/Nickel Alloy Bars Inconel 738LC K438 Nickel Alloy Round Bar](https://img2.grofrom.com/pabriktiang/fd2a87d7ae693dd24c4e05f4345ca1a9.webp)
Product Range
We have
1. Inconel series: Inconel600, Inconel 601, Inconel 625, Inconel690,Inconel718, InconelX-750, Inconel713C,Inconel738LC,N0660,N06601,N06625,N06690,N07718,N07750,2.4816,2.4851,2.4856,2.4642,2.4668,etc,
2.Incoloy series: Incoloy800H, Incoloy800, Incoloy800HT,Incoloy825,Incoloy901, Incoloy925, Incoloy926,A286,N08800,N08810,N08811,N08825,N09925,N08926,1.4980,1.4876,2.4858,1.4529,etc
3.Hastelloy series: HastelloyB, Hastelloy B-2, Hastelloy C-4, Hastelloy C-22, Hastelloy C-276, HastelloyC2000,HastelloyX,N10001,N10665,N06455,N06022,N10276,N06200,N06002,2.4617,2.4610,2.4602,2.4819,2.4675,2.4665,etc
4.Monel series:Monel400, Monel K500, N04400,N05500,2.4360,2.4375,etc
5.Pure Nickel series: Nickel200, Nickel 201, Nickel270,N02200,N02201,N02270,2.4060,2.4061,etc
6.Nitronicseries:Nitronic50,Nitronic60,Nitronic80,Nitronic105,Nitronic115,S20910,S21800,XM-19,Alloy218,etc
7.Alloyseries:Alloy20,Alloy20CB3,Alloy28,Alloy31,Alloy59,N08020,N08028,N08031,N06059,2.4605,2.4660,1.4562,etc
8. GH series:GH4169, GH4145, GH4105, GH4049, GH4033, GH4043,4180, GH3030, GH3536, GH3128, GH2132, GH1131,etc
9.MP35N
Applications for industrial :
1.Nuclear power,
2.Environmental protection,
3.Aerospace,
4.Chemical enterprises,
5. Oil drilling,
6.Desulfurization and denitrification,
7.Nuclear submarine,
8.others
Packing
Standard export packing, or as the customers' requirement.
![Casting Superalloy/Nickel Alloy Bars Inconel 738LC K438 Nickel Alloy Round Bar](https://img2.grofrom.com/pabriktiang/d2567b5d77920dc3e3051cc60f224fbc.webp)
Why choose us?
Our company established in 2004.More than 10 years of development,we become the leader in north China market in metal material products.We have more than 1000 tons of perennial stock.
What is our customer base?
Our customers are located in more than 80 countries and regions around the world,especially in the Middle East,Southeast Asia,South America,North America,Australia,Eastern Europe,Nordic has long-term stability of customers.
What is our advantage?
We have high quality products and professional services. Our products after SGS,BV,ISO certification. Our salesman has more than five years of experience.
What is the delivery time?
If we have stock, usually the delivery time is about 10-20 working days. If your products need to be produced, the delivery time is about 30 working days or 45 working days, or according to the factory arrangement.
What is the density of nickel?
The density of nickel is 8.902.
What is the melting point of nickel?
The melting point of nickel is 1453 degrees
1Black Finish Inconel738LC K438 Nickel Alloy Round Bar
2. Material Grade:
Inconel600/601/625/718/X-750/713C,
Incoloy800H/800/901/925/926/A286
Hastelloy B/B-2/C-4/C-22/C-276,
Monel400/K500,Nickel200/201
N02200/N02201/N04400/N05500/N06600/N06601/
N06625/N06690/N07718/N07750/N08800/N08810/
N08825/N09925/N10001/N10665/N06455/N06022/
N10276/N06200/N08020/S66286/K93600/N08367/N06059/N08904.
MP35N.etc
3.Standard: ASTM BS JIS NF DIN GB
4.Size: for the hot rolled bar, 8mm-100mm
For the forged bar, 70mm-400mm
5.Length: 500--6000mm,or other length as the customers' requirements.
6.Process: hot rolled, forged, cold drawn
7.Surface: black surface, polished surface
![Casting Superalloy/Nickel Alloy Bars Inconel 738LC K438 Nickel Alloy Round Bar](https://img2.grofrom.com/pabriktiang/fd2a87d7ae693dd24c4e05f4345ca1a9.webp)
Product Range
We have
1. Inconel series: Inconel600, Inconel 601, Inconel 625, Inconel690,Inconel718, InconelX-750, Inconel713C,Inconel738LC,N0660,N06601,N06625,N06690,N07718,N07750,2.4816,2.4851,2.4856,2.4642,2.4668,etc,
2.Incoloy series: Incoloy800H, Incoloy800, Incoloy800HT,Incoloy825,Incoloy901, Incoloy925, Incoloy926,A286,N08800,N08810,N08811,N08825,N09925,N08926,1.4980,1.4876,2.4858,1.4529,etc
3.Hastelloy series: HastelloyB, Hastelloy B-2, Hastelloy C-4, Hastelloy C-22, Hastelloy C-276, HastelloyC2000,HastelloyX,N10001,N10665,N06455,N06022,N10276,N06200,N06002,2.4617,2.4610,2.4602,2.4819,2.4675,2.4665,etc
4.Monel series:Monel400, Monel K500, N04400,N05500,2.4360,2.4375,etc
5.Pure Nickel series: Nickel200, Nickel 201, Nickel270,N02200,N02201,N02270,2.4060,2.4061,etc
6.Nitronicseries:Nitronic50,Nitronic60,Nitronic80,Nitronic105,Nitronic115,S20910,S21800,XM-19,Alloy218,etc
7.Alloyseries:Alloy20,Alloy20CB3,Alloy28,Alloy31,Alloy59,N08020,N08028,N08031,N06059,2.4605,2.4660,1.4562,etc
8. GH series:GH4169, GH4145, GH4105, GH4049, GH4033, GH4043,4180, GH3030, GH3536, GH3128, GH2132, GH1131,etc
9.MP35N
Applications for industrial :
1.Nuclear power,
2.Environmental protection,
3.Aerospace,
4.Chemical enterprises,
5. Oil drilling,
6.Desulfurization and denitrification,
7.Nuclear submarine,
8.others
Packing
Standard export packing, or as the customers' requirement.
![Casting Superalloy/Nickel Alloy Bars Inconel 738LC K438 Nickel Alloy Round Bar](https://img2.grofrom.com/pabriktiang/d2567b5d77920dc3e3051cc60f224fbc.webp)
Why choose us?
Our company established in 2004.More than 10 years of development,we become the leader in north China market in metal material products.We have more than 1000 tons of perennial stock.
What is our customer base?
Our customers are located in more than 80 countries and regions around the world,especially in the Middle East,Southeast Asia,South America,North America,Australia,Eastern Europe,Nordic has long-term stability of customers.
What is our advantage?
We have high quality products and professional services. Our products after SGS,BV,ISO certification. Our salesman has more than five years of experience.
What is the delivery time?
If we have stock, usually the delivery time is about 10-20 working days. If your products need to be produced, the delivery time is about 30 working days or 45 working days, or according to the factory arrangement.
What is the density of nickel?
The density of nickel is 8.902.
What is the melting point of nickel?
The melting point of nickel is 1453 degrees
material grade | UNS | GB/T 14992 | GB/T 15007 | DIN | JIS | ||
Nickel200/Ni200 | N02200 | 2.4060 | |||||
Nickel201/Ni201 | N02201 | 2.4061 | |||||
Nickel270/Ni270 | N02270 | ||||||
Monel400 | N04400 | 2.4360 | |||||
Monelk500 | N05500 | 2.4375 | |||||
Inconel600/Alloy600 | N06600 | NS3102 | NS312 | 2.4816 | NCF600 | ||
Inconel601/Alloy601 | N06601 | NS3103 | NS313 | 2.4851 | |||
Inconel625/Alloy625 | N06625 | NS3306 | NS336 | 2.4856 | NCF625 | ||
Inconel690/Alloy690 | N06690 | NS3105 | NS315 | 2.4642 | |||
Inconel718/Alloy718 | N07718 | GH4169 | GH169 | 2.4668 | |||
Inconel725/Alloy725 | N07725 | ||||||
Inconel738LC/Alloy738 | K438 | K38 | |||||
Inconel X-750/AlloyX-750 | N07750 | GH4145 | GH145 | 2.4669 | NCF750B | ||
Incoloy A286/Alloy286 | S66286 | GH2132 | GH132 | 1.4980 | SUH660 | ||
Incoloy800/Alloy800 | N08800 | NS1101 | NS111 | 1.4876 | NCF800 | ||
Incoloy800H | N08810 | NS1102 | NS112 | 1.4876 | |||
Incoloy800HT | N08811 | 1.4876 | |||||
Incoloy825/Alloy825 | N08825 | NS1402 | NS142 | 2.4858 | NCF825 | ||
Incoloy925/Alloy925 | N09925 | ||||||
Incoloy926/Alloy926 | N08926 | 1.4529 | |||||
Hastelloy B | N10001 | NS3201 | NS321 | ||||
Hastelloy B-2 | N10665 | NS3202 | NS322 | 2.4617 | |||
Hastelloy C-4 | N06455 | NS3305 | NS335 | 2.4610 | |||
Hastelloy C-22 | N06022 | NS3308 | - | 2.4602 | |||
Hastelloy C-276 | N10276 | NS3304 | NS334 | 2.4819 | |||
Hastelloy C-2000 | N06200 | NS3405 | 2.4675 | ||||
Hastelloy X/Alloy X | N06002 | GH3536 | GH536 | 2.4665 | |||
Alloy 20/Alloy 20cb/Carpenter cb3 | N08020 | NS1403 | NS143 | 2.4660 | |||
GH4049 | GH49 | 2.4636 | |||||
GH4033 | GH33 | ||||||
GH4043 | GH43 | ||||||
GH3030 | GH30 | 2.4983 | |||||
GH1131 | GH131 | ||||||
F15 | 4J29 | 1.3912 | EMAS-1001 | ||||
4J33 | |||||||
Invar36 | K93600 | 4J36 | 1.3912 | ||||
3J21 | |||||||
3J58 | |||||||
904L | N08904 | 1.4539 | |||||
AL6XN | N08367 | ||||||
Alloy59 | N06059 | 2.4605 | |||||
Nictronic50 | S20910 | ||||||
Nictronic60 |